Product
Heat Treatment Service » Heat Treatment supporting Equipments
" Pro-Vision has applied high technology heat treatment services with high precision and impeccable quality from Hitachi Metals Group. According to each type of material, size or shape, we will adopt the most suitable heat treatment program .Heat treatment technology was developed by Hitachi Metals Group can tweak the cooling speed in the temperature of different areas of the cooling process to create a balance between toughness and deformation, which always a dilemma for heat Treatment "

| 1. HARDNESS TESTER MACHINE | |
![]() |
1.1 Mitutoyo-810 ARK 601 Description
|
|
|
|
![]() |
1.2 SATO (HSD check)
|
|
|
|
![]() |
1.3 Multifunction hardness tester: HRC, HV, HSD...
|
|
|
|
| 2. GRAPHIC RECORDER MACHINE | |
![]() |
Description: Chino Corporation
|
|
|
|
| 3. HANDLING TEMPERATURE CHECKING | |
![]() |
|
|
|
|
| 4. PRINTER MACHINE | |
![]() |
Description With this tool we can send to customer the QUality indexs directly, as:
While we check the Cargos Quality. we can print the result directly |
|
|
|
| 5. MICROSCOPE | |
![]() |
- Maker: NIKON |
|
|
|
| 6. MÁY ĐO ĐỘ CỨNG TẾ VI (VICKER HARDNESS) | |
![]() |
- Maker: SHIMAZDU |